Oven Cavity Case Study

Project Scope
Replace competitive, synthetic stamping fluid to reduce/eliminate bleed out defects in porcelain enameling process.

Results
IRMCO eliminated all residue and bleed-out issues & further optimized the application process to yield further cost savings.

IRMCO’s IMPACT

  • Eliminated residue associated cleaning/enameling defects.
  • Eliminated bleed-out in porcelain enameled cavities.
  • Reduced concentration of lubricant in stamping process by 10%.
  • Optimized application process – reducing amount of applied lubricant by at least 15%.

Material
I-F Enameling steel coil – 0.0540” (1.37mm) thickness.

Product Used
IRMCO FLUIDS® 080-00B @ 6:1 dilution ratio (14.3%).

Ask an Expert